Nanoindentation characterization of polymer nanocomposites for elastic and viscoelastic properties: Experimental and mathematical approach

Gaurav Arora, Himanshu Pathak
ISSN / E-ISSN
— / —
DOI
10.1016/j.jcomc.2020.100103 ↗
Volume · Issue · Pages
4 · — · 100103-100103
Publisher
Elsevier BV
Article URL
https://doi.org/10.1016/j.jcomc.2020.100103 ↗
Article details
Unverified
Publication date (each date has its type and source)
31 Dec 2020
OpenAlex publication date · source: OpenAlex
Dates on record for this article
TypeDateSource
OpenAlex publication date31 Dec 2020 OpenAlex

Keywords (as given): polymer nanocomposites; nanoindentation; viscoelasticity; elastic properties; microwave processing; microwave power; polypropylene nanocomposites; hardness; modulus; plasticity index

HEC Status at Publication Not the journal's current status

HEC Status at PublicationNot conclusive
Best available information, not a definitive status: HEC status cannot be determined for this date: no HEC list is recorded as in effect on it.
Journal
Composites Part C: Open Access
Publication date used
31 Dec 2020 (OpenAlex publication date)
Applicable HEC period
None recorded for this date
Category
—
Recognition status
Unknown (NO_PERIOD_FOR_DATE)
Source
—
Verification status
Not available
This is an automatically generated summary based on the information available on the publication date. Terms & conditions apply.